Surface Area: 2.4 m2/g Nominal Composition: (La0.8Sr0.2)0.95Fe0.6Mn0.3Co0.1O3
|
|
|
|
Surface Area: 9.3 m 2/g Particle Size (d50): 0.25 µm Nominal Composition: La0.6Sr0.4FeO3-d
|
|
|
|
Current Stock: 1.3 Kg
|
|
|
|
Surface Area: 7.2 m 2/g Particle Size (d50): 0.36 µm Nominal Composition: La0.90MnO3-d
|
|
|
|
Surface Area: 220 m2/g Nominal Composition: Sm0.15Ce0.85O2-d
|
|
|
|
Powder suitable for tape casting, ink manufacture, pellet pressing and other non-aqueous manufacturing processes
|
|
|
|
Formulation: Various available
Surface Area: Various available
|
|
|
|
Technology: SOFC Electrolyte Powder
Formulation: La0.80 Sr0.20 Ga0.80 Mg0.20 O3- Surface Area: 4-8 m2/g Particle Size (d50): 0.3 to 0.6 µm.
|
|
|
|
Technology: SOFC Cathode Powder
Surface Area: 12.0 +/- 2.0 m2/g Particle Size: 0.30 +/- 0.20 µm. Formulation: Mn1.5 Co1.5 O4-
|
|
|
|
Technology: SOFC Cathode Powder
Surface Area: 12.0 +/- 2.0 m2/g Particle Size: 0.30 +/- 0.20 µm. Formulation: La0.60 Sr0.40 Fe O3-d
|
|
|
|
Technology: PEMFC, Direct Ethanol FC, DMFC, Direct Glycerol FC, Electrolysers and Ammonia Rewforming
|
|
|
|
Technology: SOFC Electrolyte Powder
Surface Area: 12.0 +/- 2.0 m2/g Particle Size: 0.30 +/- 0.20 µm. Formulation: La0.60 Sr0.40 Co0.20
|
|
|
|
Technology: SOFC Electrolyte Powder
Surface Area: 12.0 +/- 2.0 m2/g Particle Size: 0.30 +/- 0.20 µm. Formulation: La0.80 Sr0.20 MnO3-
|
|
|
|
Technology: SOFC Electrolyte Powder
Surface Area: 12.0 +/- 2.0 m2/g Particle Size: 0.30 +/- 0.20 µm. Formulation: Sm0.20 Ce0.80 O2-
|
|
|
|
Technology: SOFC Electrolyte Powder
Surface Area: 12.0 +/- 2.0 m2/g Particle Size: 0.30 +/- 0.20 µm. Formulation: Gd0.10 Ce0.90 O2-
|
|
|
|
Technology: SOFC Cathode Powder
Surface Area: 5-9 m2/g 50% by weight (La0.8 Sr0.2) Mn 03-x 50% by weight (Y2O3)0.08(ZrO2)0.92
|
|
|
|
Technology: SOFC Electrolyte Powder
Surface Area: 8-11 m2/g Particle Size (d50): 0.5-0.7 µm
Formulation: (ZrO2)0.90 (Sc2 O3)0.10
|
|
|
|
Technology: SOFC Electrolyte Powder
Surface Area: >100 m2/g
Primary crystallite size: 5-10 nanometers
Secondary particle size: softly agglomerated
Formulation: Gd0.10 Ce0.90 O2-
|
|
|
|
Technology: SOFC Paste
Formulation: (La0.60 Sr0.40)0.995 (Co0.20
|
|
|
|
Applications: Reducing Ink/Paste viscosity for brush-painting, spraying or other reduced viscosity deposition methods
|
|
|
|
Technology: SOFC Anode Powder
Surface Area: 3-7 m2/g
Partial Size: d50 .5 - 1.5 micrometers
|
|
|
|
Technology: SOFC Electrolyte Powder
Surface Area: >100 m2/g
Primary crystallite size: 5-10 nanometers
Secondary particle size: softly agglomerated
Formulation: Gd0.10 Ce0.90 O2-
|
|
|
|
Technology: SOFC Electrolyte Powder
Surface area: 10-12 m2/g
Particle Size: (d50): 0.5 to 0.7 µm
Formulation: (Sc2O3)0.1(CeO2)0.01(ZrO2)0.89
|
|
|
|
Technology: SOFC Cathode Paste
Formulation: 50% by weight (La0.60 Sr0.40) (Co0.20 Fe0.80) O3-x, 50% by weight (Ce0.9Gd0.1) O1.95
Solids content is 65-75 % by weight
|
|
|
|
Technology: SOFC Cathode/Anode Powder
Formulation: (Y2O3)0.08 (ZrO2)0.92 Surface area: >100 m2/g Primary crystallite size: 5-10 nanometers Secondary particle size: softly agglomerated
|
|
|
|
Technololy: SOFC Electrolyte Powder Formulation: Gd0.10 Ce0.90 O2- Surface area: 5-8 m2/g Particle Size (d50): 0.3 to 0.5 µm
|
|
|
|
Technology: SOFC Electrolyte Powder
Formulation: Gd0.10 Ce0.90 O2- Surface area: 30-40 m2/g Particle Size (d50): 0.3 to 0.5 µm
|
|
|
|
Technology: SOFC Cathode Paste
Formulation:50% by weight (La0.80 Sr0.20) Mn 03-x, 50% by weight (Y2O3)0.08(ZrO2)0.92 Solids content is 60-70 % by weight
|
|
|
|
Technology: SOFC Cathode Powder
Formulation: La0.80 Sr0.20 Mn O3- Surface area: 4-8 m2/g Particle Size (d50): 0.3 to 0.6 µm
|
|
|
|
Technology: SOFC Cathode Powder
Formulation: 50% by weight (La0.80 Sr0.20) Mn 03-x, 50% by weight (Ce0.9Gd0.1)O1.95 Surface area: 3-7 m2/g
|
|
|
|
Technology: SOFC Anode Materials
|
|
|
|
Technology: SOFC Anode Powder
Surface Area: Not more than 1 m2/g Partial Size: d50 12-22 microns
|
|
|
|
Technology: SOFC Cathode Paste
Formulation: 50% by weight (La0.80 Sr0.20) Mn 03-x, 50% by weight (Ce0.9Gd0.1)O1.95 Solids content is 65-75 % by weight
|
|
|
|
Technology: Fuel Processing Cataylst
|
|
|
|
Technology: SOFC Anode Powder
Composition: 66% NiO - 34% Sc10SZ by weight Surface Area: 4-9 m2/g
|
|
|
|
Technology: SOFC Anode/Cathode Powder
Formulation: Gd0.10 Ce0.90 O2- Surface area: 30-40 m2/g Particle Size (d50): 0.3 to 0.5 µm
|
|
|
|
Technology: SOFC Anode Materials
Formulation: (La0.80 Sr0.20) Mn 03-x Solids content 62-72% by weight
|
|
|
|
Technology: SOFC Electrolyte Powder
Surface area 13-19 m2/g
|
|
|
|
Technology: SOFC Electrolyte Powder
Formulation: Gd0.10 Ce0.90 O2- Surface area: 5-8 m2/g Particle Size (d50): 0.3 to 0.5 µm
|
|
|
|
Technology: SOFC Anode Powder
Composition: 66% NiO - 34% YSZ8 by weight Surface Area: 4-8 m2/g
|
|
|
|
Technology: SOFC Anode/Cathode Materials
Formulation: Sm0.15 Ce0.85 O2- Surface area: >100 m2/g Primary crystallite size: 5-10 nanometers Secondary particle size: softly agglomerated
|
|
|
|
Technology: SOFC Electrolyte Powder
Formulation: (Y2O3)0.08(ZrO2)0.92 Surface area: 3-7 m2/g Particle Size (d50): 0.9-1.2 µm; d80 <5 µm
|
|
|
|
Technology: SOFC Electrolyte Powder
Formulation: (Y2O3)0.08 (ZrO2)0.92 Surface area: 10-15 m2/g Particle Size (d50): 0.3 to 0.5 µm; d80 <1 µm
|
|
|
|
Technology: SOFC Electrolyte Powder
Formulation: Gd0.10 Ce0.90 O2- Surface area: 30-40 m2/g Particle Size (d50): 0.3-0.5 µm
|
|
|
|
Technology: SOFC Anode Powder
Composition: 60% NiO - 40% GDC10 by weight Surface Area: 4-8 m2/g
|
|
|
|
Technology: Fuel Proceesing Catalyst
Specs: Reforming of Methanol at 400 - 600°C
|
|
|
|
Technology: SOFC Anode/Cathode Materials
Specs: 2mm diameter, 3-4mm long
|
|
|
|
Technology: SOFC Anode/Cathode Materials
Specs: 20, 25 and 35 mm
|
|
|
|
Technology: SOFC Anode/Cathode Powder
Formulation: Gd0.10 Ce0.90 O2- Surface area: 5-8 m2/g Particle Size (d50): 0.3 to 0.5 µm
|
|
|
|
Technology: SOFC Electrolyte Powder
Formulation: Gd0.10 Ce0.90 O2-
Surface area: 30-40 m2/g
Particle Size (d50): 0.3 to 0.5 µm
|
|
|
|